air-conditioner, air-conditioner & air-conditioner helps :-) Have
never seen any reticulation.
I have access to an ice machine and do sometimes coat on a sheet of
glass on top of a developer tray filled with ice to speed up /
improve gelling. Not shure if this really is neccesarily, but it
brings the coating down to about 17ûC & there is some days when the a-
con struggles.
Tokyo
On Nov 30, 17 Heisei, at 9:00 AM, conTact wrote:
> Hi,
> who's got experience working with carbon transfer in warm
> environments (25¡C and up)?
> I could get temperatures down to around 23-24¡C with air-
> conditioning, what are major problems under these circumstances,
> reticulation of the gel?
>
> Thanks for inspirations.
>
> Sidney
______
http://halvor.deviantart.com/
http://halvor.deviantart.com/gallery/
_______________________________________________
Post to the list as PLAIN TEXT only - no HTML
carbon mailing list
carbon@spitbite.org
FAQ at http://spitbite.org/carbon/list.html
Received on Tue Nov 29 18:19:42 2005
This archive was generated by hypermail 2.1.8 : Tue 31 Jan 2006 - 02:21:47 PST